タイトル |
粘土鉱物のカリ固定とpHとの関係
|
タイトル |
The Relationship between pH and K-Fixation of the Clay Minerals
|
タイトル 読み |
ネンド コウブツ ノ カリコテイ ト PH トノ カンケイ
|
著者 |
小柴 尚博
佐野 豊
|
収録物名 |
島根農科大学研究報告
|
巻 | 12 |
開始ページ | (A)43 |
終了ページ | 45 |
収録物識別子 |
ISSN 05598311
|
内容記述 |
その他
The purpose of the experiment, described in this paper, is to examine the effect of pH on the fixation of applied K in clay minerals, namely, kaolinite, sericite, hydrated halloysite, montmorillonite. The clay minerals were adjusted to pH values ranging from 3.00 to 9.08, adding HCL or NaOH, and a constant level of KCL were added, and were dried and wetted alternately or stood at 30℃ for 48 hours. The results obtained were as follows :
1) As to kaolinite, there was no tendency in K-fixation influenced by the pH under moist condition or alternately dried and wetted conition. 2) As to hydrated halloysite, the amounts of fixed K showed the maximum at pH 5-6 under both conditions, and reduced at pH value below or above 5-6. 3) As to sericite, the amounts of fixed K increased as the pH value rose, in both conditions. 4) As to montmorillonite, the amounts of fixed K reduced as the pH rose, at pH value below 5.05, under alternately dried and wetted condition, and there was little deviation of the fixed K at pH value above 5.05. Under moist condition, there was little deviation of the fixed K caused by pH. |
言語 |
日本語
|
資源タイプ | 紀要論文 |
出版者 |
島根農科大学
The Shimane Agricultural College
|
発行日 | 1964-01-10 |
アクセス権 | オープンアクセス |
関連情報 |
[NCID] AN00108241
|
備考 | A,Bを含む |