粘土鉱物のカリ固定とpHとの関係

島根農科大学研究報告 Volume 12 Page (A)43-45 published_at 1964-01-10
アクセス数 : 1083
ダウンロード数 : 400

今月のアクセス数 : 95
今月のダウンロード数 : 7
File
d0020012n009.pdf 431 KB エンバーゴ : 2002-07-03
Title
粘土鉱物のカリ固定とpHとの関係
Title
The Relationship between pH and K-Fixation of the Clay Minerals
Title Transcription
ネンド コウブツ ノ カリコテイ ト PH トノ カンケイ
Creator
Koshiba Naohiro
Sano Yutaka
Source Title
島根農科大学研究報告
Volume 12
Start Page (A)43
End Page 45
Journal Identifire
ISSN 05598311
Descriptions
The purpose of the experiment, described in this paper, is to examine the effect of pH on the fixation of applied K in clay minerals, namely, kaolinite, sericite, hydrated halloysite, montmorillonite. The clay minerals were adjusted to pH values ranging from 3.00 to 9.08, adding HCL or NaOH, and a constant level of KCL were added, and were dried and wetted alternately or stood at 30℃ for 48 hours. The results obtained were as follows :
1) As to kaolinite, there was no tendency in K-fixation influenced by the pH under moist condition or alternately dried and wetted conition.
2) As to hydrated halloysite, the amounts of fixed K showed the maximum at pH 5-6 under both conditions, and reduced at pH value below or above 5-6.
3) As to sericite, the amounts of fixed K increased as the pH value rose, in both conditions.
4) As to montmorillonite, the amounts of fixed K reduced as the pH rose, at pH value below 5.05, under alternately dried and wetted condition, and there was little deviation of the fixed K at pH value above 5.05.
Under moist condition, there was little deviation of the fixed K caused by pH.
Language
jpn
Resource Type departmental bulletin paper
Publisher
島根農科大学
The Shimane Agricultural College
Date of Issued 1964-01-10
Access Rights open access
Relation
[NCID] AN00108241
Remark A,Bを含む